Q47
Cold cracking in the heat affected zone of a high strength steel weld can take place because of the
A.
Retained austenite
B.
Martensite formation
AnswerC.
Relatively high sulphur content in the base metal
D.
Sufficient hydrogen present in the welding arc
Answer: Option B
Solution
Answer: Option B
No explanation is given for this question Let's Discuss on Board