Q7
In a hardening process, the hypo-eutectoid steel is
A.
Heated from 30°C to 50°C above the upper critical temperature and then cooled in still air
B.
Heated from 30°C to 50°C above the upper critical temperature and then cooled suddenly in a suitable cooling medium
AnswerC.
Heated from 30°C to 50°C above the upper critical temperature and then cooled slowly in the furnace
D.
Heated below or closes to the lower critical temperature and then cooled slowly
Answer: Option B
Solution
Answer: Option B
Solution:
In a hardening process, the hypo-eutectoid steel is Heated from 30°C to 50°C above the upper critical temperature and then cooled suddenly in a suitable cooling medium