Loss on ignition (LOI) of iron ore is determined by finiding the loss in weight of the sample by heating it first to 500°C for 5 minutes followed by its heating at . . . . . . . . °C, for 30 minutes.

A.
250
B.
750
C.
950
Answer
D.
1150

Answer: Option C

Solution

Answer: Option C
No explanation is given for this question Let's Discuss on Board