Q25
Match the corrosion phenomenon with the material in which they are commonly observed. P. Season cracking 1. 70 : 30 brass Q. Pitting corrosion 2. GI water line fitted with a brass tap R. Galvanic corrosion 3. Duralumin S. Caustic embrittlernent 4. Boiler steel
Match the corrosion phenomenon with the material in which they are commonly observed.
| P. Season cracking | 1. 70 : 30 brass |
| Q. Pitting corrosion | 2. GI water line fitted with a brass tap |
| R. Galvanic corrosion | 3. Duralumin |
| S. Caustic embrittlernent | 4. Boiler steel |
A.
P-1, Q-2, R-3, S-4
AnswerB.
P-4, Q-3, R-2, S-1
C.
P-1, Q-2, R-4, S-3
D.
P-3, Q-4, R-1, S-2
Answer: Option A
Solution
Answer: Option A
No explanation is given for this question Let's Discuss on Board