Pick out the wrong statement.

A.
Etal/alloys having hexagonal crystal lattice structure are less malleable than those having cubic crystal lattice structure
B.
Etal/alloys having body centred cubic (bcc) crystal lattice structure is stronger & less ductile than those having face centred cubic (fcc) crystal lattice structure
C.
Ungsten has a body centred cubic (bcc) crystal lattice structure
Answer
D.
Oth ferritic & austenitic stainless steel has a face centred cubic (fcc) crystal structure

Answer: Option C

Solution

Answer: Option C