Vidyalelo
Metallurgical Engineering · Q4

Physical Metallurgy

Engineering and GATE · Metallurgical Engineering · question 4

Q4

A 0.4 wt% C steel is austenitised at 900°C for 1 hour and heat treated to get different. inicrostructures. Match the following microstructures to the heat treatments. P. Martensite + Retained austenite 1. Annealing Q. Ferrite + fine pearlite 2. Quenching R. Ferrite + spheroidal cementite 3. Quenching + temperature at 600°C S. Ferrite + coarse pearlite 4. Normalising

A 0.4 wt% C steel is austenitised at 900°C for 1 hour and heat treated to get different. inicrostructures. Match the following microstructures to the heat treatments.
P. Martensite + Retained austenite 1. Annealing
Q. Ferrite + fine pearlite 2. Quenching
R. Ferrite + spheroidal cementite 3. Quenching + temperature at 600°C
S. Ferrite + coarse pearlite 4. Normalising
A.
P-4, Q-3, R-2, S-1
B.
P-1, Q-2, R-3, S-4
C.
P-2, Q-4, R-1, S-3
D.
P-2, Q-4, R-3, S-1
Answer

Answer: Option D

Solution

Answer: Option D
No explanation is given for this question Let's Discuss on Board