Vidyalelo
Metallurgical Engineering · Q149

Physical Metallurgy

Engineering and GATE · Metallurgical Engineering · question 149

Q149

Match the following fractographic features with the type of fracture with which they are associated. P. Striations 1. Ductile fracture Q. Separated grain facets 2. Brittle fracture R. Dimples 3. Fatigue fracture S. Facets, river pattern 4. Intergrannular fracture

Match the following fractographic features with the type of fracture with which they are associated.
P. Striations 1. Ductile fracture
Q. Separated grain facets 2. Brittle fracture
R. Dimples 3. Fatigue fracture
S. Facets, river pattern 4. Intergrannular fracture
A.
P-3, Q-4, R-1, S-2
Answer
B.
P-3, Q-4, R-2, S-1
C.
P-4, Q-3, R-2, S-1
D.
P-1, Q-2, R-3, S-4

Answer: Option A

Solution

Answer: Option A
No explanation is given for this question Let's Discuss on Board