Q118
Match the following. Group-I Group-II P. Hot shortness 1. Overcome by adding excessive amount of manganese Q. Cold shortness 2. Weld decay R. Season cracking 3. Reduction in impact strength at low temperatures S. Sensitization 4. Tendency of brasses to corrode due to high residual stress
Match the following.
| Group-I | Group-II |
| P. Hot shortness | 1. Overcome by adding excessive amount of manganese |
| Q. Cold shortness | 2. Weld decay |
| R. Season cracking | 3. Reduction in impact strength at low temperatures |
| S. Sensitization | 4. Tendency of brasses to corrode due to high residual stress |
A.
P-1, Q-3, R-4, S-2
AnswerB.
P-4, Q-3, R-2, S-1
C.
P-1, Q-3, R-2, S-4
D.
P-1, Q-2, R-3, S-4
Answer: Option A
Solution
Answer: Option A
No explanation is given for this question Let's Discuss on Board