Vidyalelo
Mechanical Engineering · Q190

Manufacturing And Production Technology

Engineering and GATE · Mechanical Engineering · question 190

Q190

Two streams of liquid metal which are not hot enough to fuse properly result into a casting defect known as

A.
Cold shut
Answer
B.
Swell
C.
Sand wash
D.
Scab

Answer: Option A

Solution

Answer: Option A
No explanation is given for this question Let's Discuss on Board