Which one of the following microstructures of a Ni-base superalloy imparts the highest creep resistance?
A.
Fine grained equiaxed
B.
Coarse grained equiaxed
C.
Columnar
D.
Single crystal
AnswerAnswer: Option D
Solution
Answer: Option D